/en-US/products-services/accessories /en-US/products-services/products
close-up of shiny metallic, cylindrical precision parts with holes

Quality control of solid materials

Base decisions on solid science

 

Delve into the process of improving quality throughout production

 

Manufacturing teams use our latest measurement technology to make swift, data-driven decisions before and after coating, printing and bonding. From polymers, composites, glass, and metal to wood and other natural materials see how surface science drives quality control.

What is your material?

What is your process?

Top View Analyzer – TVA100B for wetting measurements in depressions

TVA100B

Wetting measurements in depressions and on concave surfaces

Top View Analyzer

Why test inks cannot tell the full truth about surface free energy

A comparative study between test inks and contact angle measurements in our laboratory

Application Report

Mobile Surface Analyzer – MSA One-Click SFE for wettability analysis

MSA Flexible Liquid

Fast, automatic, and non-destructive wetting analysis with your liquids of choice

Mobile Surface Analyzer

finger tapping on the touchscreen of a tablet

Coating of glass

Quality control of the interface chemistry of glass bonds and treated surfaces

Use Case

Drop Shape Analyzer – DSA25B for contact angle

DSA25B

The easy-to-use manual instrument for changing contact angle tasks

Drop Shape Analyzer

Drop Shape Analyzer – DSA25E for wettability measurement and adhesion

Replacing the solid needle by a liquid one when measuring static contact angles

Comparison of the traditional solid needle dosing system and a novel pressure-based dosing system, a …

Application Report

Circle method

Method for determining the contact angle in drop shape analysis. With the circle method (circular segment …

Glossary

Modern bathroom with white tub, toilet, cabinet and black towel on towel rack.

Production of ceramic surfaces

Methods for optimizing the surface of ceramic materials and coatings

Use Case

Liquid Needle

The Liquid Needle is a dosing technology for optical contact angle measurement developed by KRÜSS.

Glossary

hands wearing gloves working with a golden, round silicon wafer

Quality control of wafers

Contact angle and surface energy as parameters for the structure of homogenous, functional wafer layers

Use Case

Drop Shape Analyzer – DSA100L for wettability analysis of large samples

DSA100L

Automatic wettability analysis of large surfaces

Drop Shape Analyzer

close-up of a person putting in a contact lens

Wettability of contact lenses

Contact angle measurements for ensuring quality and the development of biocompatible materials

Use Case

close-up of the red bumper light of a dark gray car

Coating of polymers

Methods for measuring wetting and adhesion

Use Case

close-up of white, gray, and black carbon fibers

Fiber reinforced polymers

Contact angle and surface tension for optimizing the wetting and adhesion between fibers and matrix …

Use Case

metal plates are immersed in a cleaning bath

Determine how clean surfaces are: Quickly and on the go

Optimizing residence times in cleaning baths

Application Report

Models of hip and knee joints with metallic prosthetic implants

Biocompatibility of medical implants

Surface characterization for body-compatible dental and bone prostheses

Use Case

automatic dispensing system applies adhesive to a cell phone frame

Adhesion on polymers

Contact angle and surface tension for optimizing plastic coatings

Use Case

Ayríís

Surface quality control has never been so easy and reliable

Portable contact angle instrument

Height-width method

Method for determining the contact angle in drop shape analysis. The contact angle is calculated from …

Glossary

Top-view distance method

The top-view distance method is an optical method for measuring the contact angle.

Glossary

Surface free energy (SFE), surface energy

Surface free energy (SFE) is the work that would be necessary to increase the surface area of a solid …

Glossary

Characterizing particle size of filler materials quickly and easily

Sedimentation measurements on calcium carbonate powders with a tensiometer

Application Report

Drop Shape Analyzer – DSA30S for wettability analysis

DSA30S

The versatile instrument for semi-automatic wettability analysis

Drop Shape Analyzer

Why test inks don’t tell the full truth

One of the most commonly used methods to approach surface free energy is test …

Online

Webinars & Seminars

Moving Beyond Cross Hatch: The Stood-Up Drop Technique as a New Route to Assess Coating Adhesion

Correlating the dewetting angle with ISO2409:2020 test results

Application Report

woman lathering and washing her hair

Optimizing Shampoo Foam Analysis: A Comparative Study of Measurement Techniques

Evaluating the effectiveness of Sparging, Foam Flash, and Adapted Foam Flash

Application Report

Roll-off angle

The roll-off angle is the angle of inclination of a surface at which a drop rolls off it.

Glossary

paint brush applies a protective varnish to a brown wooden surface

Surface treatment of wood

Surface tension and contact angle for optimizing the protection and bonding of wood

Use Case

Surface Science Online Course

Increase your knowledge and update your practical expertise in the field of surface science. Facilitated …

Online

Webinars & Seminars

Wettability

Wettability describes the attempt of a solid to form a common interface with a liquid which comes into …

Glossary

Drop Shape Analyzer – DSA25S for wettability measurements

DSA25S

Semi-automatic wettability analysis with high dosing precision

Drop Shape Analyzer

Bricklayer's trowel with mortar lies on stacked hollow concrete blocks

Production of cement and concrete

Interfacial chemistry measuring methods for the material behavior before and after setting

Use Case

print heads on a large-format digital printing machine produce blue and white colour patterns_2

Inkjet printing

Optimization of the ink, the printing process and the substrate with surface science methods

Use Case

yellow paint is applied to a white wooden wall with a brush

Paints and varnishes on surfaces

From spreading, adhesion, interfacial tension to the final functions of the finished coating

Use Case

close-up of a blue motherboard

Production of electronic boards

Optimization of cleaning and final coating using surface chemical methods

Use Case

Detailed view of a chrome multi-spoke car wheel with gold bolts and visible brake disc

Metal plating

Interfacial measurement techniques for characterizing wetting agents and checking for their concentration

Use Case

Owens, Wendt, Rabel and Kaelble (OWRK) method

The Owens, Wendt, Rabel and Kaelble method is a standard method for calculating the surface free energy …

Glossary

soldering iron soldering a small component onto a green circuit board

Soldering processes

Contact angle and surface tension as parameters for optimizing soldering processes

Use Case

close-up of a blue UV curing lamp in a printing press

Offset printing

Quality assurance by means of interfacial chemical investigations of moistening agents, inks and printing …

Use Case

Interfacial tension

In the broader sense, interfacial tension is defined as the work which must be expended to increase …

Glossary

Lotus effect

The lotus effect (lotus blossom effect) describes the behavior of ultrahydrophobic surfaces.

Glossary

Surface roughness

Surface roughness is the degree of unevenness of the surface of a solid below the scale of magnitude …

Glossary

robotic arm paints the bodywork of a blue car

Coating of metals

Chemical interface measurements for protection, painting and bonding

Use Case

two plasma torches generate a bright, radiant arc on a surface.

Polymer surface treatment

Contact angle measurements for determining wettability and adhesion

Use Case

close-up of crisscrossing white glass fibers

Coating of fibers

Methods for monitoring wetting, adhesion and cleaning

Use Case

Sessile Drop

The sessile drop is the standard arrangement for optical measurement of the contact angle using drop …

Glossary

Drop Shape Analyzer – DSA30B for contact angle

DSA30B

The versatile manual instrument for changing contact angle tasks

Drop Shape Analyzer

Tensiometer

A tensiometer is a device for measuring the surface tension of a liquid and/or the interfacial tension …

Glossary

Close-up view of a car interior showing the steering wheel, start button, air vent, and dashboard controls

Optimizing flame treatment of polymer surfaces

Mobile contact angle measurements on glass fiber reinforced composite materials for automobile interiors

Application Report

hand wearing a latex glove operates a touchscreen

Production of latex

Investigations into the wetting of immersion molds and into dispersion and emulsion stability

Use Case

Spreading

Spreading describes the expansion of a liquid phase on a second liquid or solid phase (complete wetting). …

Glossary

Drop Shape Analyzer – DSA100W for wettability and adhesion on wafers

DSA100W

Automatic wettability and adhesion analysis of wafers and other round samples

Drop Shape Analyzer

Wetting

Wetting describes the degree to which a liquid spreads on a solid when it comes into contact with it. …

Glossary

DSA100E

The automated premium solution for wetting and adhesion analysis of solids and liquids

Drop Shape Analyzer

DSA30E

Versatile automated wetting and adhesion analysis of solids and liquids

Drop Shape Analyzer

Polar part

The polar part is that part of the surface free energy of a solid or the surface tension of a liquid …

Glossary

industrial robotic arm paints a hood with blue paint

Adhesion on metals

Contact angle and surface tension for the processing of metal surfaces

Use Case

Contact angle

When an interface exists between a liquid and a solid, the angle between the surface of the liquid and …

Glossary

Drop Shape Analyzer – DSA100B for contact angle

DSA100B

The manual premium solution for changing contact angle tasks

Drop Shape Analyzer

Drop shape analysis

Drop shape analysis (DSA) is an image analysis method for determining the contact angle from the shadow …

Glossary

Mobile Surface Analyzer – MSA One-Click SFE for wettability analysis

MSA One-Click SFE

Analyzing wettability in a second with only one click

Mobile Surface Analyzer

Confocal microscopy

Confocal microscopy is an optical method for obtaining three-dimensional images of surface textures …

Glossary

Drop Shape Analyzer – DSA25E for wettability measurement and adhesion

DSA25E

From one-click wettability measurement to analysis of solid-liquid adhesion

Drop Shape Analyzer

Car glass factory

Adhesion on glass

Contact angle and surface tension in glass cleaning and coating

Use Case

water droplets rolling off a blue rain jacket

Wetting and coating of textiles

Contact angle and surface tension for optimizing the coating of functional textiles

Use Case

Drop Shape Analyzer – DSA100S for wettability analysis

DSA100S

The semi-automatic premium solution for wettability analysis